dc.contributor.advisorVildoso Flores, Alejandro
dc.contributor.authorCanales Portaro, Fernando Antonio
dc.date.accessioned2022-08-11T23:24:31Z
dc.date.available2022-08-11T23:24:31Z
dc.date.issued2021-06-30
dc.identifier.citationCanales, F. A. (2022). Análisis de la resistencia a la compresión axial y diagonal de un muro de mampostería y mortero de concreto con añadido de 2%, 4% Y 6% de virutas de acero reciclado. Lima 2021 [Tesis de licenciatura, Universidad Privada del Norte]. Repositorio de la Universidad Privada del Norte. https://hdl.handle.net/11537/31126es_PE
dc.identifier.other624.153 CANA 2022es_PE
dc.identifier.urihttps://hdl.handle.net/11537/31126
dc.description.abstractLa presente tesis tuvo como objetivo realizar el análisis comparativo de la resistencia a la compresión axial y diagonal del muro de mampostería con mortero tradicional versus la adición con 2%, 4% y 6% de viruta de acero reciclado, para lo cual, se ensayaron en laboratorio 84 muros de dimensiones 0.60 x 0.60 m, escogiéndose una muestra de 36 muros para ensayo axial y 48 muros para ensayo diagonal, a edades de curado: 7, 14, y 28 días. El instrumento de medición fue la observación directa, ya que permite ser metódico en cuanto al cumplimiento a pie de letra con el cronograma para recolección de datos: recolección de virutas de acero reciclado, pruebas de los ensayos realizados para la obtención de las propiedades mecánicas de los muros de mampostería tradicional y muros de mampostería utilizando mortero de concreto con añadido de virutas de acero reciclado, según la norma ASTM 140/NTP 399.604. Como conclusión, se tiene que, a los 28 días de curado la resistencia a la compresión axial añadiendo el 2% de viruta de acero reciclado resulta ser más eficiente al muro con mortero tradicional, mientras que añadiendo el 4% la eficiencia es similar al tradicional y con el 6% resulta ser menos eficiente al diseño tradicional. Por otra parte, la resistencia a la compresión diagonal añadiendo el 2% de viruta de acero reciclado resulta ser más eficiente al muro con mortero tradicional, sin embargo, los diseños del 4% y 6% resultan ser menos eficientes que el diseño tradicional.es_PE
dc.description.abstractThe objective of this thesis was to carry out a comparative analysis of the axial and diagonal compressive strength of the masonry wall with traditional mortar versus the addition with 2%, 4% and 6% of recycled steel shavings, for which, in the laboratory 84 walls with dimensions 0.60 x 0.60 m, choosing a sample of 36 walls for axial test and 48 walls for diagonal test, at curing ages: 7, 14, and 28 days. The measurement instrument was direct observation, since it allows to be methodical in terms of compliance to the letter with the schedule for data collection: collection of recycled steel shavings, tests of the tests carried out to obtain the mechanical properties of traditional masonry walls and masonry walls using concrete mortar with the addition of recycled steel shavings, according to the ASTM 140/NTP 399.604 standard. In conclusion, after 28 days of curing, the axial compressive strength adding 2% of recycled steel shavings turns out to be more efficient than the wall with traditional mortar, while adding 4% the efficiency is similar to the traditional one. and with 6% it turns out to be less efficient than the traditional design. On the other hand, the diagonal compressive strength by adding 2% recycled steel shavings turns out to be more efficient than the traditional mortared wall, however, the 4% and 6% designs turn out to be less efficient than the traditional design.es_PE
dc.description.uriTesises_PE
dc.formatapplication/pdfes_PE
dc.formatapplication/mswordes_PE
dc.language.isospaes_PE
dc.publisherUniversidad Privada del Nortees_PE
dc.rightsinfo:eu-repo/semantics/openAccesses_PE
dc.rightsAtribución-NoComercial-CompartirIgual 3.0 Estados Unidos de América*
dc.rights.urihttps://creativecommons.org/licenses/by-nc-sa/3.0/us/*
dc.sourceUniversidad Privada del Nortees_PE
dc.sourceRepositorio Institucional - UPNes_PE
dc.subjectMuroses_PE
dc.subjectResistencia a la compresiónes_PE
dc.subjectMortero (Materiales de construcción)es_PE
dc.subjectConstrucciónes_PE
dc.subjectAnálisis comparativoes_PE
dc.subjectReciclajees_PE
dc.subjectMasonry wales_PE
dc.subjectResistance to axial and diagonal compressiones_PE
dc.subjectMortar with additiveses_PE
dc.titleAnálisis de la resistencia a la compresión axial y diagonal de un muro de mampostería y mortero de concreto con añadido de 2%, 4% Y 6% de virutas de acero reciclado. Lima 2021es_PE
dc.typeinfo:eu-repo/semantics/bachelorThesises_PE
thesis.degree.grantorUniversidad Privada del Norte. Facultad de Ingenieríaes_PE
thesis.degree.levelTítulo Profesionales_PE
thesis.degree.disciplineIngeniería Civiles_PE
thesis.degree.nameIngeniero Civiles_PE
dc.publisher.countryPEes_PE
dc.subject.ocdehttps://purl.org/pe-repo/ocde/ford#2.01.01es_PE
thesis.degree.programPregradoes_PE
dc.description.sedeBreñaes_PE
renati.advisor.dni10712728
renati.advisor.orcidhttps://orcid.org/0000-0003-3998-5671es_PE
renati.author.dni73202414
renati.discipline732016es_PE
renati.jurorNeyra Torres, Jose Luis
renati.jurorManturano Chipana, Ruben Kevin
renati.jurorVereau Miranda, Edmundo
renati.levelhttps://purl.org/pe-repo/renati/level#tituloProfesionales_PE
renati.typehttp://purl.org/pe-repo/renati/type#tesises_PE


Ficheros en el ítem

Thumbnail
Thumbnail
Thumbnail
Thumbnail

Este ítem aparece en la(s) siguiente(s) colección(ones)

Mostrar el registro sencillo del ítem

info:eu-repo/semantics/openAccess
Excepto si se señala otra cosa, la licencia del ítem se describe como info:eu-repo/semantics/openAccess